Fast Clean Purge
INJECTION MOLDING
Injection
Molder Machine 1300 ton class / Material: PP resin running at 428OF
After
purging all remaining material from barrel, 11 lbs. of Fast
CleanTM 250 is introduced into the machine.
1.
Picture one depicts purging of old material (one cycle depicted
per photo. Approximately 2 lbs. of material purged
per cycle). Fast
CleanTM 250 is then placed into the injection
machine.
2.
Fast CleanTM begins to exit the nozzle
exhibiting a "wavey" appearance.
3.
Third to fourth shot, purged Fast CleanTM
begins to change color.
4.
Fourth to fifth shot, the old material color is nearly gone.
5.
By the seventh or eigth shot, approximately 8-9 lbs. of Fast
CleanTM has passed through the machine cleaning
both burnt residue and old material from cylinder.
6.
By the ninth or tenth shot, Only Fast CleanTM
is exiting the machine exhibiting it's original color with no
contaminants.
ONE
SHOT = 40 SECONDS / COLOR CHANGEOVER OR CLEANING TIME 6 MINUTES
|